Monday, December 18, 2017

Re: [MW:27199] stress by analysis

Dear Ramin.
yes you are right .Von Mises or Tresca is used in DIV I,II. but it just limited to primary stress(general membrane stress) not combination with other categories of stress.

Regards.

On Sunday, December 17, 2017 at 1:41:42 PM UTC+3:30, Ramin Kondori wrote:
Most of these are based on calculating Maximum Distortion Energy. Von Mises is a normal (and simplistic) approach to specify such criteria. 

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small

On Sun, Dec 17, 2017 at 9:39 AM, Ali Asghari <asghar...@gmail.com> wrote:
Dear All.

Does any body know or introduce some references about reason& philosophy of  stress limits for combination of all categories of strees?for example 3S for combination of primary and secondary stresses.(especially in ASME VIII DIV II)

Regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...