Saturday, October 7, 2017

Re: [MW:26883] Weld overlay PD5500

Dear abhisek,

Probably not, you need to ask your customer.

Some customer allowes it.

Regards,
Brajendra Patel


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of ABHISHEK SINGH <mech.abhi17@gmail.com>
Sent: Saturday, October 7, 2017 5:28:07 PM
To: Materials & Welding
Subject: [MW:26879] Weld overlay PD5500
 
Dear Experts,

In my Job construction code is PD5500. Can I use Overlay  PQR qualified as per ASME Sec. IX instead of EN15614-7??

Regards
Abhishek Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Think before you print. This e-mail may contain confidential and privileged material for the sole use of the intended recipient. Any review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive for the recipient), please contact the sender by reply e-mail and delete all copies of this message. Koso India Pvt Ltd. --- H-33 & 34, MIDC, Ambad, Nashik – 422010, Maharashtra, India ,Tel + 91 253 2408811, Fax + 91 253 2384413
Think before you print. This e-mail may contain confidential and privileged material for the sole use of the intended recipient. Any review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive for the recipient), please contact the sender by reply e-mail and delete all copies of this message. Koso India Pvt Ltd. --- H-33 & 34, MIDC, Ambad, Nashik – 422010, Maharashtra, India ,Tel + 91 253 2408811, Fax + 91 253 2384413

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...