Saturday, October 7, 2017

Re: [MW:26882] Weld overlay PD5500

In general not accepted
However compare the qualifying variables if matching explain for the acceptance

Thanks and Regards
Sathiyanarayanan

> On 07-Oct-2017, at 2:58 PM, ABHISHEK SINGH <mech.abhi17@gmail.com> wrote:
>
> Dear Experts,
>
> In my Job construction code is PD5500. Can I use Overlay PQR qualified as per ASME Sec. IX instead of EN15614-7??
>
> Regards
> Abhishek Singh
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...