You need to know about the design codes of the equipment to perform NDT inspection, for example:

 

ASME B31: For piping and pipelines

ASME VIII: For pressure vessels

AWS: For structure, D1.1 Carbon steel, D1.2 Aluminum, etc.

 

In some cases specific codes apply, for example API for oil & gas, NBIC for pressure vessels, etc.

 

Previous NDT you need to read the "Scope Chapter" of each code, standard, norm or reference document, and you will find relevant information where the document apply: materials, thicknesses, kind of structure, limitations, etc.

 

Best Regards…

 

J. Clemente

 

De: 'Shashank Vagal' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Enviado el: mar
tes, 12 de septiembre de 2017 07:43 a. m.
Para: materials-welding@googlegroups.com
Asunto: Re: [MW:26815] Acceptance Criteria

 

Sec VIII has limited application, only for pressure vessels.

 

Best Regards,

Shashank C Vagal  

 

 

On Tuesday, 12 September 2017 12:08 AM, Somnath Ashtakar <s.ashtakar@gmail.com> wrote:

 

Please refer the ASME SEC VIII.... You will get the answer over there..

 

On Fri, Sep 8, 2017 at 9:26 AM, Vijay Joshi <hivijay1970@gmail.com> wrote:

Friends,

Many time for some odd jobs, we find the contractor is not clear on what is acceptable when NDT is conducted.

For example, we had to UT some welds on a repaired columns of a gantry crane.

There was no reference Code of construction.

Therefore, will you please help me in knowing what Codes are applicable to what type of jobs and what is their respective acc criteria references?

Thanks,

Vijay

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.



 

--

Thanks and Regards,
Somnath Ashtakar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...