Saturday, September 2, 2017

Re: [MW:26786] Reg:suitable filler wire

Smooth grind it and perform Pickling & Passivation standard ASTM A380
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677



From: Gopi Nath <gosri2813@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, September 2, 2017 6:50 AM
Subject: [MW:26784] Reg:suitable filler wire

Dear sir,
I had find weld spatches after welding in machined valve body .  This  is not accepted. Material ASTM A487 Gr 4C. Need your solution
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...