Monday, September 11, 2017

[MW:26814] Welder qualifications

Dear all,
Pls.let me know material P1 qualify Welder can weld P11 if yes how or no how, for eg. P no., F no. , as I know P1 to P15F qualification range as per sec IX

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.