Monday, August 21, 2017

Re: [MW:26731] Welding of 316L pipe with F347 flange

I do not see any dilution problem. Normally dilution will be 70% from welding consumable and 15% from either side of the Base Metal. You can use electrode E316L or E347. I forsee the problem due to Molybdenum segregation due to wrong parameters.

Since this is dissimiar weld, where the Mo in 316L plays a role in improving Pitting corrosion resistance, still there are chances to accept provided other Alloying elements meeting the requirement.
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677



From: "biju.psl@gmail.com" <biju.psl@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sunday, August 20, 2017 5:22 PM
Subject: [MW:26730] Welding of 316L pipe with F347 flange

Hi,
We have a to weld a 316L pipe to F347 flange using 316L electrode.after welding during PMI it has been noted that Mo content in weld metal is only 0.15--0.21 range.Is there any document which specifies how much dilution can be acceptable

Biju
Sent from my iPad

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...