Thursday, August 10, 2017

Re: [MW:26711] Permanent attachments welded on shell after hydro test by contractor

10" 

On Tue, Aug 8, 2017 at 4:22 AM, Kishor Swaminathan <kishors28@gmail.com> wrote:
Dear Pinto,

What is the Size of the Nozzles.

Thanks
Kishor


On Sat, Aug 5, 2017 at 10:55 AM, Pinto Antony <pintoantony81@gmail.com> wrote:
Dear All,

We are constructing 2 tanks at the site, after the hydro test the subcontractor team cut one nozzle on above HHL and the supports of the same nozzles are welded with pad plate on the shell at the below level of the hydro test. what is your opinion?? they did not inform us and the Owner.


Thanks

Pinto 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Kind Regards

PINTO ANTONY.T

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...