Presume the weld is  F91 to it self ( P= 15E  to P15E) where you require to follow certain welding discipline
i.e. Preheat -> Welding continuously  not below preheat temp->Post heat at about 300-320C (If asked by client spec)-> cool below 100C to convert to martensetic sructure -> later PWHT as per Code say 730-760C  Then only you will get hardness between 190-260BHN which is generaly acceptable limit

(If SMAW E9015 B9 is used with lower H control)

Regards
Hegde P.b.


On Friday, 4 August 2017 5:37 PM, mmm <mustaqnk@gmail.com> wrote:


Seal weld joint between bonnet and body
1)Weld deposit thickness is 8mm.
2)design code- API-602
3)Electrode - E9015-B91
4)base material for bonnet and valve
  body- SA 182 Gr F91
5)hardness of the weld joint is 300 BHN.

Dear experts
a)Please let me know what are method to reduce the Hardness of the weld joint?
b) is this electrode is correct or not please specify if its wrong

Thank you.
MNK

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...