Thursday, August 31, 2017

[MW:26777] Hardness unit

Dear Experts,

We are using the MH310 Leeb Hardness Tester to check the hardness of the piping weld joints ( For production- NACE material) . Project specification states that the maximum allowable value is 248 HV10. When using the MH310  Tester to check, the Tester only shows the unit HV (not specified HV10). Client QC worry about unit of value:  the HV unit displayed is HV10 or HV. HV/HV10 are equivalent ? Client required to clarify.

Please help me to clarify this issue and give reference.

Thank you so much.

 

GIGI

Piping Inspector

 

 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...