Sunday, August 20, 2017

[MW:26730] Welding of 316L pipe with F347 flange

Hi,
We have a to weld a 316L pipe to F347 flange using 316L electrode.after welding during PMI it has been noted that Mo content in weld metal is only 0.15--0.21 range.Is there any document which specifies how much dilution can be acceptable

Biju
Sent from my iPad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]