Sunday, June 25, 2017

Re: [MW:26645] ASME Tack welder Qualification

There is no specific tack welders qualification. If tack welds are performed by non qualified welders they have to be grinded off



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Karunakaran Pasupalagovindasamy <pgkaruna@doosan.com>
Date: 23/06/2017 13:26 (GMT+02:00)
To: materials-welding@googlegroups.com
Subject: [MW:26639] ASME Tack welder Qualification

Dear Experts,

Is there any ASME clause for Tack welder qualification?

Kindly share the input.

 

Regards,

Karunakaran. P.G.

 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...