ER 70S-2 has 70,000 psi UTS, where E 6013 is with 60,000 psi.

No idea about you line pressure. it could be app. 7 kg/cm2. Pl. check.

ER 70S-2 with E 7018 can be a better choice.


From: Mahek Shah <mahekshah03@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 19 June 2017 6:28 PM
Subject: Re: [MW:26622] WQT- Electrode

Dear Expert,

Shall I weld the ER 70S2 as root welding and 6013 as a final welding in my compressor pipe line?

Regards,
Mahek shah

On Mon, Jun 19, 2017 at 1:53 PM, SHIVARATRI SHANKAR <sshankar.irs@gmail.com> wrote:
WPS needs to be established please.

Thanks & Regards,
Shankar Shivaratri,
Hyderabad, India.
Mobile : +91 9346970604


On 14 June 2017 at 23:42, Perumal Govindan <perumalgovindan@gmail.com> wrote:
Hi
Please let me know what are the approved WPS you are having.
Find out also the scope of your work is piping or pipeline.
Regards
P Govindan
On Jun 14, 2017 07:12, "Shankar S" <sshankar.irs@gmail.com> wrote:
Dear experts,

At one particular LPG bottling plant contractor proposed  WQT approval root run as E6010 and fill as E7010.  I have doubt that E7018 is suppose use for fill up only. 

Project: Pipeline. Pipe specification PSL2( API)-  Oil & Gas. Ref. standards: API 1104, ASME B 31.4/8.

Please suggest accordingly.

Thanks in Advance.

regards,
Shankar
Hyderabad India.
--
https://materials-welding.blog spot.com/
https://www.linkedin.com/group s/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/grou p/materials-welding.
For more options, visit https://groups.google.com/d/op tout.
--
https://materials-welding.blog spot.com/
https://www.linkedin.com/group s/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/grou p/materials-welding.
For more options, visit https://groups.google.com/d/op tout.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...