Dear Jiju ; 

Please check your specification for usage of 6010, in my previous project it was not allowed due to HICC. 

Regards; 

Demir Alp ILIKOBA 

On Sat, Jun 3, 2017 at 8:36 AM, Sundaraj Anish <anishsundaraj@gmail.com> wrote:
Dear friend,

 You can use E6010 for root and E7018 for other passes, Otherwise check your Tender specification

On Thu, Jun 1, 2017 at 11:48 AM, jiju balan <jj@arcube.in> wrote:
dear team,
what electrode should be used to weld  API 5L GR-B PSL1 pipes.

regards

On Wednesday, January 2, 2013 at 5:32:43 PM UTC+5:30, krishna wrote:
Dear Team,

We have WPS/PQR for SA106 Gr.B(P1-P1) whether this shall be used for welding of API 5L PSL2
seamless & welded pipes for production and welder qualification.

pls share your experiences.

thanks,
krishna

Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Thanks & regards

Anish S 

Sr.Engineer-QA/QC

Corrtech International Pvt Ltd

Kochi

Mob: +91 9442938358

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...