Friday, June 9, 2017

[MW:26604] Re: ASME B31.3 -2014 Table 331.1.1 Soaking time for P1 material


Dear Sirs

Kindly take a look





On Monday, May 29, 2017 at 7:03:46 AM UTC-3, SWI wrote:
Hi Team,

Could any please clarify
What is the minimum required soaking time for P1 material with wall thick 12mm, as per ASME B31.3 year 2014 Table 331.1.1 .

Is it still Minimum one hour per 1 Inch wall thickness or Minimum 15 Minutes...


Regards,

Ram

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...