Sunday, April 16, 2017

Re: [MW:26425] Regarding Post Heating or Post Baking

Check in ISO 1011-2

On 11-Apr-2017 10:08 AM, "Mohit Aggarwal" <aggarwalmohit05@gmail.com> wrote:
Dear Experts,

Kindly share the standard or code in which there is mention about post Heating of Alloy Steep materials like 
SA 335 P5 and SA 335 P9 etc.

Regards,
Mohit Aggarwal
9821958461

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPNOQS0jNPgxPwQgmMY1bn4WLnG2x00WsFVN%3DPuFC9U37Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNOqc7nDgX%3D-%3D%3DeMHXg2AifGV8MSOv6NMWVPr%3DFvvoOJg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...