[MW:26424] recommended filler Wire for hastelloy D-205 to Alloy-20 Weld

Dear Experts,

 

Need your expert advice on following subject matter.


Attaching herewith the chemical composition of hastelloy D-205 &  Alloy-20(UNS N08020)

 

We want to seal weld between these dissimilar metal  for elimination of leakage.

 

Kindly suggest recommended filler Wire & weld parameter for the same.



Thanks & regards,

Brajendra Patel

Cont:+917057406907




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bi%2BCirf9wVr4kKJ_bQ38Un1Sg1s8my387XU%3Ddqfg0rFQpcuFQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...