Friday, March 24, 2017

Re: [MW:26278] Re: SA 387 Gr. 11

  1. with what method that I need to use when I want to Joint Plate for Type material like SA-387 Gr. 11 to SA 516 Gr. 70. and what kind of Electrode that I need to use? is it enough using ER 80S B2 in Gtaw?
Yes, but take when PWHT, be on the lower side of the temperature range
  1. Similiar to question above, What Kind of method that I will use when want to join material Plate like SA240 Gr. 304H to SA-387 Gr. 11?
When PWHT: butter Gr. 11 with 2 layers on Inconel 625, do PWHT, remachine (or grind) weldbevel  and make final weld with Inconel, without PWHT
No PWHT: preheat to 120 degrees centigrade and weld with either 309 wire or Inconel 625, beware of interpass for Inconel being 150 degrees, also limit heat input to 1.2 kJ/mm
 
Regards  
Weld-Tech vof
 
Ir. J. Prinsen IWE
Member of IWCR
 

Van: "Materials & Welding" <yudistira.dunggio@gmail.com>
Aan: "Materials & Welding" <materials-welding@googlegroups.com>
Verzonden: Vrijdag 24 maart 2017 08:41:24
Onderwerp: [MW:26277] Re: SA 387 Gr. 11

Is there anyone in this group can help wme with my situation??

regards
Yudistira

Pada Kamis, 23 Maret 2017 13.22.31 UTC+7, Materials & Welding menulis:
Hai All,

I'm knew in this group.
I believe many of you have many expereince in this situation.

I've been try to looking many refferences but still hard to find the right one.

my Problem are:

  1. with what method that I need to use when I want to Joint Plate for Type material like SA-387 Gr. 11 to SA 516 Gr. 70. and what kind of Electrode that I need to use? is it enough using ER 80S B2 in Gtaw?
  2. Similiar to question above, What Kind of method that I will use when want to join material Plate like SA240 Gr. 304H to SA-387 Gr. 11?

perhaps many of you can help me on this situation.

Thank you for your information on this

Warm regards
Yudistira

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/40d1827e-f356-43e6-804e-4404cdf4d316%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...