Wednesday, March 22, 2017

[MW:26253] Welding of TP 405

Dear Experts,
please suggest the welding consumable for the combinations of materials provided below,
1. 410S to 410S - P No. 7 to P No. 7
2. SA516 Gr. 60 with TP405 Clad to SA 240 TP 405
3. SA 240 TP 405 to SA 240 TP 405 - P No. 7 to P No. 7
4. 410S to SA 240 TP 405

Regards
Anandh Kumar

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH9aXeHvjZ7v8YbE0OJbZxnV3fPSD1Y3hdsK6ik7%3DRSYizr6Yw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...