Re: [MW:26091] Welding of Low alloy to Stainless Steel

if there is not PWHT requirement thn you can start welding directly without buttering.
Otherwise you start with buttering on 5A, then you perform PWHT and then you complete the weld


2017-02-13 6:38 GMT+02:00 Shaunak Upadhyay <shanupadhyay@gmail.com>:
Dears,
 
Please give your valuable guidance.
 
I have weld joint between P5A to P8 materials, using nickel base consumable.
Before start this butt joint, is it mandatory to do buttering on P8 material ? or we can weld direct butt joint groove between these two materials. (SA387 GR22 CL2 or SA240 TP304L)
 
Thanks, 
Regards,
Shaunak Upadhyay.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD1AzTQxzQDMfnMr1%3DKJO8uYa8vQN-Ep_pn1Lh9torEHLsLEsw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CbF_GafjvPdL_NZZ8BtFecR%3DdWyrMf8e05eBnodgh05w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...