Monday, February 13, 2017

Re: [MW:26061] WELDER QUALIFICATION

thnks ..how abt ASME?.....and is RT mandatory for welder qualification??...can i use other techniques such as DPI

On Mon, Feb 13, 2017 at 10:35 AM, 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
AWS D1.1 does not cover anything less than 1.6 mm thick.
 
Best Regards,
Shashank C Vagal  (Quality Adviser)
Neo Metal-Analyst & NDT Services (Approved by IBR, Thermax, AERB)
Regd Office: 301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel: +91 22 2611 6640 / (+91) 9821386292 /  8082395502 / 9819191861    
Works Office: A-25, Geet Siddhee, Sector No. 11, Pradhikaran, Gat No. 62, Boradewasti, Moshi, Dist: Haveli, PCMC, Pune – 411044, Maharashtra, India   
www.neometalanalystndt.com / enquiry@neometalanalystndt.com nach_sam@yahoo.com







From: VISHNUDAS MAVUNKASHERY <36vishnudas@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 13 February 2017 11:22 AM
Subject: Re: [MW:26058] WELDER QUALIFICATION

thanks buddy....one more doubt plz...here we r using plates ASTM A653 G90(GI SHEETS) 1.2mm,1.5mm,2mm,3mm etc...so on which thickness should i make the test coupn for welder qualification inorder to qualify for this thickness range?

On Mon, Feb 13, 2017 at 7:49 AM, 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com> wrote:
No
Please follow your construction code



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: VISHNUDAS MAVUNKASHERY <36vishnudas@gmail.com>
Date: 12/02/2017 23:34 (GMT+05:30)
To: Materials & Welding <materials-welding@ googlegroups.com>
Subject: [MW:26053] WELDER QUALIFICATION

i have doubt..if the procedure qualification is done under ASME SECTION ..  so can i do the welder qualification under AWS D1.1 ???????.
--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
To post to this group, send email to materials-welding@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ 49a25c41-9eba-48c5-b9cd- ceabe1732f93%40googlegroups. com.
For more options, visit https://groups.google.com/d/ optout.
--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
To post to this group, send email to materials-welding@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ 39o3n8x2jjrtewuu1uwd216b. 1486957780346%40email.android. com.

For more options, visit https://groups.google.com/d/ optout.



--
VISHNUDAS MURALI MAVUNKASHERY
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK8EmDRB1BTooYjKQJ0u9Oy2Mn%3D3Z9G56xaEjE_Np5GGtHUEyw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/900389995.2874751.1486967702956%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.



--
VISHNUDAS MURALI MAVUNKASHERY

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK8EmDQ4XRNjOQZ5gzukNPHCWtb7LdsqqWzBTOKeeatZ6v1YBQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...