Saturday, January 21, 2017

Re: [MW:25965] WELDER QUALIFICATION CERTIFICATE RENEWAL AS PER ASME SEC. IX

Dear
if welder under six months then they can weld but over six months then they have re test.

a p gupta
saudi


On Sat, 21 Jan, 2017 at 2:42 PM, Manoj John
<manojacgnr@gmail.com> wrote:
Dear Friends,

We have qualified welders in groove welding (GTAW+SMAW) as per ASME section IX but they have welded 2 months butt welding and 4 months they welded only fillet joints. Now they completed 6 months and they are continuing welding.  

My question is how can we renew their certificates since they do not have any Radiography reports for fillet joints.  Can we renew their certificate with a visual inspection report.

Thanks & Regards.

Manoj John.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nBM2QU9Uv6y98y1YLy0gpA8sbUU88XHKG0LHHaeEnZ%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1354970302.1105379.1484996275891%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...