Hi!
Generally petrochemical Ind spec
Allows logngitudinal overlay in pipe smaller than 50mm ID

 However
I)For pipe ID overlay in longitudinal way causes more distortion compared to circumferential O/lay
ii)Longitdinal O/L =difficult to maintain uniform ID after overlay hence some time recommended  to machine the ID to  achieve uniform overlay thk in pipe
Regards
Hegde


On Thursday, 8 December 2016 5:17 PM, ABHISHEK SINGH <mech.abhi17@gmail.com> wrote:


Dear experts,
      Anyone know why some of the client not allowed for overlay in longitudinal direction in nozzle I. D, PIPE I.D,Elbow I.D. Is there are any technical reason??

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/50260987-8d03-46b7-b90a-e5e9a8d29f9f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...