Tuesday, November 15, 2016

Re: [MW:25704] Fw- Tack welder quailification as per AWS D1.1

Please advice whether i can use 6mm thk plate ,T joint with 50mm fillet weld of 6mm size and break the same to check fusion.

On Tue, Nov 15, 2016 at 7:12 AM, 'c sridhar' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Or, you can qualify a tack welder with a groove joint in 1G and check the root penetration. 



From: anthony chundal <anthony.chundal@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 14 November 2016 12:35 PM
Subject: [MW:25690] Fw- Tack welder quailification as per AWS D1.1

Dear All,

Kindly advice with regards to qualifying tack welders as per AWS D1.1, 

Please let me know about tack welder qualification, its not in ASME, but in AWS it states, whether we can use plate thk of 6mm T joint and weld 50mm length of 6mm size and break the same to check the fusion , is it ok
Thanks and regards,
Anthony.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp-nUO7i4FubD5WAMFmuFT8Kr8ydY%3DKozcwcEBB%2BDqgk%2BA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1030232193.119350.1479179556470%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp_61Fren_5M_xjxd-zfHgjaMO7bkfnHm_-m1TixFS_T6Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...