Dear Kumar,

If it is E7018-1 & if impact testing is there  then the cert has to be 3.1 which will give you the tested values ,as 2.2 will only give you values as per code.

Thanks & Regards


On Oct 21, 2016 14:53, "Kumar" <sk7920541@gmail.com> wrote:
Dear Experts,

Greetings.

Requesting the views on MTCs (EN 10204 ) for electrode  ( SFA/AWS A
5.1 E 7018-1 H 4 R, 4.00mm). In fact according to project spec. it
should be 3.1. but the contractor could only provide 3.1 for chemical
& mechanical 2.2 in a single MTC.

Since its a deviation from the spec., how far this will affect the
quality of the product when mechanical according to 2.2 & chemical
according to 3.1? how this could be convinced to the end user.

Your valuable feedbacks are appreciated.

thanking in advance,
Kumar.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp9j4g08J_sEsjtQ15OF2%2BUyZh8k1v9ky8arTPB53bbVtA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp-8CFPDx4nPzRrmJ66fWM38Fk6ZK1D3KgNPZstEmkVOiw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...