Re: [MW:25381] LTCS PQR

in your case and assuming that your Code is ASME VIII-1,  A333 for this thickness & temperature  is not exempted from Impact test. What is the governing thickness of A350? You can avoid impact if you satisfy all conditions of UG-20 

2016-09-08 8:21 GMT+03:00 Mustaq Ahmad <mustaqnk@gmail.com>:
Dear Experts 

I am new for this job please help me 

for PQR of LTCS

1) required thickness min is 6.35mm &  dia is 12 inch

2) design press = 20kg/cm2
    design temp  = -45.6/37.8 degreee celcius
     op press      = 20 max
     op temp       = -40 degree celcius

3)  material is pipe - A 333 GR 6(P1 &G1) and flange - A350 GR LF2 RF

4) service is LPG plant- Relief and blow down

now please suggest me 
 a) what is is the size of the test coupon can be selected(dia with schd) where can i find the exact length of weld required to carry out mechanical testing for this PQR?
 b) is it possible to carry out the PQR for pipe to flange joint 
 c) what consumable can be selected for this if GTAW & SMAW ?
 

Regards
AHMAD

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1dff4f26-85ba-4a9d-a731-d037ac27bea3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D9BP_YMVf2TSL098RxpNzX9%3Dgk1O7XMwUXYq%3DRuQeQcQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...