Dear Expert,

Need your guidance,

I have PQR with P1 to P43 with 10 mm thickness,

Can i use this PQR for Joint with 10 mm (P1) & 45 mm (P43) under following clause?

Clause no QW 202.4.



Thank you 

Vijay Katkar   

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrLBSmMTdd95CHbS3q5oiP_%3DRfqYAwUR9EK%3DyGH4xHJYTQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...