[MW:25407] Requirements of PWHT Offshore Jacket Pipe

Dear Experts,


Good Morning,


We are having our own project to build an offshore jacket for a depth of 15 to 20 meter water depth. For this project we are in the stage to order the material (PIPE) from the Steel Mill. In order to start the process the mill is asking for the SPEC of PWHT. So can anyone able confirm what should be the Holding temp / time / No of cycle / Stress relieving cycle required for PWHT.


Sl.No

Material Size

Grade

Remark

1

24" Pipe x 25mm wall thick

API 5L Gr.X52N PSL2

Normalizing Steel

2

30" Pipe x 30 mm wall thick

API 2H GR.50 +(Z35)

Normalizing Steel

3

20" Pipe x  25mm wall thick

API 5L Gr.X52M PSL2

TMCP Steel

 

 


Regards

Thandesh

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABatnw_-jRk6uM_CiFVFgT5YQHSQM1FuWRsV6kzykJPWhUVQeQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...