Re: [MW:25278] Welder qualification

Dear Krisanu Bhunia and Experts,


FOR WELDER QUALIFICATION TEST


I would like to share my experience as below, ( correct me if I am wrong. )


From Quality point of View:

·         First thing is " Welder qualification test" is done to determine the ability of a welder

to deposit sound weld metal.

·         Sound metal means a quality weld at first time. ( without making visual defects like cracks, undercuts, porosity, excess reinforcement, Etc. )

·         As per ASME SEC IX, the only visual criteria you could find as mentioned below:

·         QW-194 Visual Examination — Performance

Performance test coupons shall show complete joint

penetration with complete fusion of weld metal and base

metal.


From Production Point of View: -  During the test, If a welder making undercut or with Visual porosity – please reject him, before your client does the same, since this welder if qualified  - he will make more undercuts and porosity in the Job and uses grinder repeatedly / wastes precious time schedule of the project / off course increase the work of Welding Inspector and cannot make a productive output results. Hope you got the message.


AND FINALLY – Client have to decide !


Regards,


Sathish

Jazan, Saudi.


On Sun, Aug 21, 2016 at 12:12 AM, Krisanu Bhunia <krisanu.bunty@gmail.com> wrote:
Daer.ALL
Please tell me cluster porosity acceptance limit for Welder qualification test as per ASME XI or VII.

 Regards
krisanu bhunia

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMZth3rV_ULUn4hEhHvtKAKuzQD5i4t5sFXcCZvZ%3DWHZQN40mA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bh6G00a9nQ-9fHaEXQSxZqKAn-hGyU7TyjnGDBwbgS-Sao%2BGw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...