Re: [MW:25248] Pitting corrosion test failure

Hi Prasad

Please let me know the exact material spec and welding consumable brand used for welding.

Further what was the max interpass temp measured, shielding and purging gas used and its flow rates.

Regards
Govindan Perumal

On 11 Aug 2016 09:30, "Prasu Cutie" <pracuty@gmail.com> wrote:

Dear experts,

We had pittng corrosion failure in duplex stainless  steel 2205
Process: GTAW
Thk: 7.62mm
Filler: ER2209
Product: pipe
Heat input observed: 1.5 to 2.5kj
Gas: argon 99.9997purity
Weight loss reqd is <4g/sq.mtr, achieved 21g/sq.mtr
Testing is done as per ASTM G48

Can any one tell me why this failure occured, what could be the reason?

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKgcArS8ogq8UVK8TnByOg9L7Garxaej2a1pwHyQ8iR9MeSRuQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9d%2BwoQtAxKiWnUxPg15c8ZM1TZPFgUYgNGgR7uLG6H14Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...