Tuesday, August 16, 2016

[MW:25260] RE: 25250] STUD AND BOLT

Hi – when it comes to minimum, as per code some are refereeing to one thread, some are two thread, and some are three thread…

But your question is very tricky…

 

Understand the concept, bolts are intended to keep hold the parts together and as pet that No of threads in engagement will be decided and confirmed by the designer as per standard…

 

To ensure that all the threads are in engage – evidence of the engagement is that minimum one or two threads has to out from the nut.

 

But maximum is as per your convenience and application and situation…

 

If more threads comes out (Means stud length more),

It might get interfere with other equipment and place constrain is an issue.

Or else might be difficult to place the stud as the stud length is more.

Or threads may get rusted, and will difficult while removing the nut for a lengthy stud portions..

Or stud cost will be more…

Or operation & maintenance cost will be more (u have to prevent from rusting the stud threads, and applying compound for it regularly when it comes to sea environment and all)

Or more time for tightening and loosening (during break down  time)

 

Like as so many other parameters will influence the situation…

There is no code defining for maximum length of threads come out from the nut…

As an engineer we should decide accordingly…

 

 

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sundaraj Anish
Sent: Saturday, August 13, 2016 9:18 AM
To: materials-welding@googlegroups.com
Subject: [MW:25250] STUD AND BOLT

 

Dear experts,

I have a query and looking  for earliest  response

How many threads should protrude beyond the nut?

 

 minimum 3 threads and maximum how many threads ?

 

Awaitng for your  response

Thanks & regards

Anish S 

Engineer-QA/QC

Mott MacDonald Pvt Ltd

Hassan

Mob: +91 9442938358

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtc4G5ccCSktoX3iRe_3WOgjJgiZUXPo6Jc3HuW%3D4Oa8YMTAQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...