Monday, July 18, 2016

Re: [MW:25113] PWHT

Dear Sir,

Please mention where it is in See viii ?

On Sun, Jul 17, 2016 at 8:36 PM, José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
It is assumed that in making this repracion of welding after the PWHT is no longer necessary to repeat again PWHT, but this is only for numbers P1 and P3 under certain thicknesses with the Building Code BPVC ASME Section VIII Div. 1

At this point I do not have exactly the reference code, you send it later for your review it thoroughly.

2016-07-17 0:18 GMT-05:00 Krisanu Bhunia <krisanu.bunty@gmail.com>:
Thanks, but is it possible to avoid PWHT ?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8b07bebe-fb05-458a-b2bb-1eafd1d993bd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8116171750

Skype: jjjimeneza

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/uHRzkNOaGNw/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLrs1RcFQMkx6YPMPLMMp%3Dypi%2B1i3kTyy7ZnD7LaZRMig%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMZth3pTzRgbmpU6542YAWZgKmaM5vULUE0iRe%3DnZ1BHi5Fx_g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...