Re: [MW:25109] PWHT

According to Section VIII Div. 1 BPVC ASME, you can do some kind of repracion after the PWHT welded, but this only applies to materials P1 and P3 number and for some thicknesses, which clearly defines the code.



2016-07-16 6:31 GMT-05:00 syed moinul hasan <mhsyed1@gmail.com>:
After PWHT, if the welding is added , that means  you have to discard residual stresses which occured  due to additional  welding.
Hence, you have to go for Re-PWHT , refernce ASME 31.3

On 15 July 2016 at 01:41, Krisanu Bhunia <krisanu.bunty@gmail.com> wrote:
Dear sir,

In clean out door in tank we found welding not sufficient after PWHT.(A 537 CL1)
SO, now need to welding again . PWHT again doing or can avoid it by which code ?

Regards
krisanu bhunia
 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMZth3qmH8a3w0Efd96-M12HsymvR61YRPz18j1nOFpdZME9PQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMXKe_rAhWor%2B-ESFSSYX9sJ3-G1vJBLwCf3b0rjNN_uAJHaQA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8116171750

Skype: jjjimeneza

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJRfJrJb1Qbi%2BANiEt_w1t5L%2BCgEKa7uEsULeibEwf60g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...