Tuesday, July 12, 2016

Re: [MW:25092] Type of metal transfer

as per ur data, u will get only globular. u can also get shortcirciut but since ur thick is 40mm ,do not opt for shortcircuit which may lead to coldlap

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Mon, Jul 11, 2016 at 3:53 PM, udaya bhaskar <dusroni@gmail.com> wrote:

sir what you are said that is for low thickness up to 3 mm we were used dip or short circuit transfer, but here at 40 thk

On Jul 11, 2016 14:27, "Alan Denney" <alan@denney1.freeserve.co.uk> wrote:

Correction: generally we use short circuit transfer.

 

Alan Denney

 

 

From: zs00765@rediffmail.com [mailto:zs00765@rediffmail.com]
Sent: 10 July 2016 08:08
To: materials-welding@googlegroups.com
Subject: Re: [MW:25080] Type of metal transfer

 

Dear
There are three types of metal transfer.
Short circuit ... Lower voltage...18-20v
Globular... Medium voltage ... 20 _24v
Spray... Above 24v all are approximately.

Generally in welding we adopt globular or spray transfer.

Sent from RediffmailNG on Android

From: "udaya bhaskar"dusroni@gmail.com
Sent:Sun, 10 Jul 2016 11:54:01 +0530
To: materials-welding@googlegroups.com
Subject: [MW:25079] Type of metal transfer


Hi dear all,


>

PLEASE CLARIFY IN WHICH MODE OF METAL TRANSFER WE DONE  WELDING ? .


>

FOR WPS

 

MATERIAL : IS2062 E250BR


>

THICKNESS: 40 mm


>

PROCESS : GMAW(MAG)


>

GAS          : 100 % CO2


>

MODE OF METAL TRANSFER : ?

--
>

With Regards


>

Udyabahaskar.D


>

+919951728551

--
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3ROShqy3BJdZ57HboYJEpZ9jo1Lq%3DDMJzHoRQfGVyBm4Bg%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.
>

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1468131841.S.10149.26987.f5-224-116.1468134487.21063%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000f01d1db0d%24e868b8d0%24b93a2a70%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM52_aFM943RcnS1C5U-JUJmvzGmonvt-mtwjjq1P7XMw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMtQKAbA75Z%2Bcbht3MGY3%3Dzx0_VhNs%2BqrWoTGYHQ2BUPQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...