Friday, July 15, 2016

[MW:25103] RE: 25098] Pull out test

Depends on project requirements but normally not location of fracture but minimum pull out load is specified.

 

Met vriendelijke groeten / Best Regards,

 

Herman Pieper

QA-QC Inspector / CSWIP + IWI-C Welding Inspector / IWT / Materials Expert

 

Job van der Havestraat 6

8384 DB, Wilhelminaoord

Cell: +31 6 51691215

 

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Chokshi Darshan
Verzonden: dinsdag 12 juli 2016 16:42
Aan: Welding Group <materials-welding@googlegroups.com>
Onderwerp: [MW:25098] Pull out test

 

During pull out test in mock up of tube to  tubesheet  joints,
If it is broken from tube then it is acceptable or broken from weld is acceptable?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BEr1RfwRcTAHB9VpPihWo1vrcS_qd3LLPeOuqvrt17E-AGGgQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...