[MW:25083] Re: Type of metal transfer

Also it's not possible to see spray transfer with %20 or more CO2.



10 Temmuz 2016 Pazar 09:24:01 UTC+3 tarihinde dusroni yazdı:

Hi dear all,

PLEASE CLARIFY IN WHICH MODE OF METAL TRANSFER WE DONE  WELDING ? .

FOR WPS
 
MATERIAL : IS2062 E250BR

THICKNESS: 40 mm

PROCESS : GMAW(MAG)

GAS          : 100 % CO2

MODE OF METAL TRANSFER : ?
--
With Regards

Udyabahaskar.D

+919951728551

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ae285ff5-d8c1-4d6e-b05b-a7d81cfa4db7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...