Thursday, June 30, 2016

Re: [MW:25036] Chang in groove angle

If it's tky joint you shall qualify in 6 gr position in accordance with d1.1

Sent from my iPhone

On Jun 30, 2016, at 9:20 AM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:

Question is for D1.1

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Wed, Jun 29, 2016 at 2:19 PM, pradip kumar Sil <pradipsil@gmail.com> wrote:
Groove design is not the essential variable as per ASME Sec IX 

On Wed, Jun 29, 2016 at 10:29 AM, shaik amjad <amjadshaik7842@gmail.com> wrote:
Dear All

I have a PQR qualified in double v bevel  can i write a wps for single v using this PQR (code is AWS D1.1).

I have a PQR qualified with double v joint , but in construction we need for TYK Joint ie single V ., So my question is can i write a WPS using this PQR nd change grove as Single V.

Regards 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ec55954a-3944-4b52-9dba-671dc324073d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3Die-6vd64fdDLsm_CamGE%2BaObH-Wc%2BDuY3QBZu958jgA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP7nhPV%3DZs%2BbdC%3DjZB%2BC0tOaJpvmCXGeazzYDNN4wWtRQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...