Decrease current
Decrease travel speed
Increase Voltage
Reduce flux burden
change over to high manganese rod
Check the flux sizes

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sun, Jun 26, 2016 at 6:40 PM, Rajesh Reddy <rajeshreddy32@gmail.com> wrote:
Hi,

Increase heat input to the maximum extent (by reducing travel speed & increasing wire speed/current).  it solves the problem

Regards,

Rajesh Reddy

On Wednesday, June 9, 2010 at 11:48:50 PM UTC+5:30, masthan wrote:

Hi

 

We are continuously facing problem of Poak marks on the SAW Welding surface. Welding Consumable L-61 (wire) with 865 (flux) combinations. Any body has idea to prevent this. Please share.

 

Best Regards

 

M.Masthan

K.S.A

 

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7d8b2e0d-8d8d-4285-a4c7-a46d63580938%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMwcAuXHJoM5Fhe6UC9f0brBPDZaB%3Db%3D%3DhMjW%2BdZ6wY_Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...