Re: [MW:24958] Impact test exemption as per B 31. 3

Impact testing is mandatory requirement for A333.

Hafiz Ali Alvi

Sent from my iPhone

On Jun 15, 2016, at 9:17 AM, 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com> wrote:

A piping spool is to be fabricated.
Construction code: ASME B 31.3

Service LPG liquid
MDMT : minus 45 degree Celsius

Client spec calls for impact requirements. 

Pipe MOC is A 333 grade 6; Size 2 inch schedule 80 and 3 inch schedule 40.

My question is are these two thicknesses of 5.54mm and 5.49mm exempt from impact testing as per B 31.3 Fig. 323.2.2A curves ??

Please provide B 31.3 code reference. 

Regards

Prem Nautiyal
9769316004


Sent from Samsung Mobile

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/w307dtxxgn6ng9cqo11020e4.1466005983348%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...