Mode of metal transfer plays a major role to choose this conventional GMAW process. If u have pulsed GMAW, in all current it will be in the pulsed spray mode only and u can use it for any thick, any position?

On 17-Apr-2016 8:10 pm, "Alan Denney" <alan@denney1.freeserve.co.uk> wrote:
Yes you can, but not outside because the gas shield gets blown away. The big issue is lack of fusion defects. I hope that you have trained welders, qualified welding procedures and non-destructive testing, and that you are working to a recognised welding code of practice.

Alan Denney
AKD Materials Consulting Ltd

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthikeyan Shanmugananthan
Sent: 14 April 2016 11:40
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24691] MIG welding process-reg

Dear Experts
Can we use MIG welding process for load carrying structural steel.... and also provide limitations of MIG welding process

Expecting your valuable suggestions

Regard
S.karthikeyan
Chennai

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d4a08674-c496-48d6-91df-9c49a35d8bd8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/002a01d19641%24b0bad550%2412307ff0%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOckJ497Y-My6Ko9g-rd2dM-wDX6Qf%2BOGOczEf2iNGRYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...