[MW:24735] Re: Regarding welding of ErNicr3 and PWHT

PWHT is must in view of Hard HAZ on GR 91 side

On Tuesday, April 12, 2016 at 7:44:31 PM UTC+5:30, Anuj Sharma wrote:
Hi everyone please suggest

We have very less constrained space for the PWHT on and we have called 4 different PWHT teams and all teams have ignored PWHT due to less space.
Our material is SSH Header 40 mm thick and P91 material ehich we have to dummy with P91 material only.
As recommended by us to use ErNiCr3 filler wire with pre heat at 220deg C and no PWHT required is it ok.
??

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/391e7db6-4704-4954-b2b8-1215e1e788ec%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...