Monday, February 29, 2016

RE: [MW:24407] Fillet weld cracks below 6 mm with suitable NDT.

After performing gauging, we found most of the cracks are below 6mm

On 29 Feb 2016 06:18, "Mohd Siraj" <mohd52100@gmail.com> wrote:
How u know crack is exactly 6mm below??

quite interesting.
Do RT.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1346669f-f39d-4460-a282-dc42b4377911%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjhGLOwWX-UqX7t3YWCO8GLEZKuiFzVcP9OHk3-Ld9VCw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...