Monday, February 29, 2016

Re: [MW:24405] RE: 24355] Impact Test & cooling Rate-Preheating (carbon steel)

in welding, lower thickness will have slow cooling  when compared to higher thickness weld which will have fast cooling rate, that is why to slowdown , preheat is applied to avoid hard structure which inferior for toughness properties

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Sat, Feb 27, 2016 at 10:21 PM, 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
One more addition to Alan's good comment:
In case of lower thicknesses, the cooling rate tends to increase and may lead to martensite formation. But it is not so slow and sustained a cooling rate as to promote grain growth/reduced ductility, as you are allowed to weld between preheat & interpass temperatures.
 
BR,
Shashank C Vagal 




From: Alan Denney <alan@denney1.freeserve.co.uk>
To: materials-welding@googlegroups.com
Sent: Tuesday, 23 February 2016 2:59 AM
Subject: [MW:24358] RE: 24355] Impact Test & cooling Rate-Preheating (carbon steel)

 
Alan Denney
AKD Materials Consulting Ltd
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohd Siraj
Sent: 22 February 2016 09:22
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24355] Impact Test & cooling Rate-Preheating (carbon steel)
 
Dear all,
 
Background: 
impact testing is more critical for less(low)thickness than higher thickness.
 
Reason  : 
fine grain form during fast cooling and course grain form during slow cooling.
 
Question is:
Preheating use to lower the cooling rate for higher thickness.
So lower the cooling rate means form the course grain,course grain lower the toughness.
 
Preheating contributing to lower the toughness?
 
 
 
 
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3247d39d-f53a-4bc4-aee8-79f73a1d95d8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003801d16db8%2430d2dab0%2492789010%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/613526275.231430.1456591879950.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM9fdE1Yu4c9%3D0bV7xkqtuHBhCK2FMMPsDbbrwhwVt17g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...