Dear All,

Please clarify below points, if have reference standard also write in your reply.

1. PQR in ASME - Certified by Manufacturer
Who can certified PQR? QC manager or welding engineer?
In my company no have welding manager. So who can certify PQR.

2. WPQ in ASME - Certified by Manufacture
Who can certified?
Same question as above.

3. WPS in ASME -
WPS require approved by QC Manager or welding engineer can approve this ?

Please reply your valuable answer and if have specific ASME clause number let me know.

Thanks in advance.

Regards
Shaunak.
shanupadhyay@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d0a84f3d-85a6-4c51-a2ec-a5ea1ae7beb5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...