Re: [MW:24013] IMPACT EXEMPTION FOR DUPLEX FLANGES SA 182 Gr F51

Thanks MW,

But my question remains same that, what will be nominal thickness of duplex flanges to be consider ?
 

vish

On Thursday, December 24, 2015 at 2:58:57 PM UTC+5:30, MW wrote:
i guess you should use Appendix JJ, 
UHA -51(g)?


On 24 December 2015 at 13:11, VISHNU <vishnu...@gmail.com> wrote:
Dear sir,

I have one query regarding to above subject,

One of the definition of governing thk when using fig. UCS-66 - Governing thickness of flat non welded parts, such as bolted flanges, tubesheet and flat head is the flat component thickness divided by 4

But what about Duplex flanges ? UHA is not giving such clause, so what will be governing thickness to be consider for duplex flanges (SA 182 F51) ?

Thanks in advance

Regards

vishnu 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/40269871-9939-415e-8563-80b29b024ff0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...