Qualification range will be pipe or plate 0,7 - 2,0 mm to plate 2,0 - 8,0 mm for single layer fillet welds. Beside that also throat thickness (á) is an essential variable (0,75 - 1,5 x á)

Op dinsdag 15 december 2015 10:34:39 UTC+1 schreef vijay Katkar:
Dear All,

Need your help,

I have qualified  fillet weld PQR with following ,

Thickness of Pipe:- 1 mm

Thickness of Plate :- 4 mm

I have confusion about base metal qualification thickness,

 Qualification thickness will be 0.7 mm to 8 mm for single layer for both Pipe & Plate

Or 

For Pipe it is 0.7 to 2 mm &  for plate it is 3-8 mm.

What is correct? 

Thank you

Vijay Katkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5d43167f-a85e-467f-b2ce-e05cf6cb3151%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...