Thursday, November 26, 2015

Re: [MW:23928] Jacket piping

Yes,

We will get reducing flanges, in sulfur lines we will be using and in chilled water/brine water jacketing also used.

On Wed, Nov 25, 2015 at 11:17 PM, PRASANTH RAJAN <prasanthgalfar@gmail.com> wrote:
Dear experts    
  Is it possible for welding of jacket outer pipe on the  the inner pipe flange , its there any standard that allow the welding of pipe in forged material


--
WITH REGARDS
 
*PRASANTH RAJAN*
*MECHANICAL SUPERVISOR*
*GALFAR ENGINEERING EMIRATES*
*prasanthgalfar@gmail.com* <prasanthgalfar@gmail.com>
 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKCULh5fjVmbvFdPkmqpg3%3DB1WNAU9v%2BfB_bkoML1p-1oiXD6w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Ohm Guru Namasivaya

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFj9zKMmATzXdTP7RfnynvTKnfiyvCR4YMyfOxMNxFi67%2BVZzw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...