Re: [MW:23911] Re: Weld Repair Procedure as per API 1104

Dear Members

    As per API1104 Latest edition below mentioned repair procedures is mandatory.

1.Full thickness repair.

2. Cover pass repair
3.Partial  thickness repair
4.Internal Partial thickness repair
5. Back weld reapir

 Note:- Refer Clause 10.3,10.3.1,10.3.2


Regards
Madhusoodhanan  Nair.G




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE12Qq70oRk9Y8jYTSGkFHy8%3DrENFPRmkmQiU1K5LzsAEMn0eQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...