Re: [MW:23900] Other Project PQR Can be used New project on Different Clients?

If use other company PQR must prove the both company relation (sister concern)
client is approval required .Same company different project no issue.
peter

On Wed, Nov 18, 2015 at 9:43 PM, dominic v.k.dominic <v.k.dominic@gmail.com> wrote:
Dear Expertise,
The contractor submitted other project PQR and approved by some other third party company and client.
My Question: Can used other client approved PQR for this new project and new Client?
In the code (API-1104 and ASME Section -IX) anywhere specified in this matter for Employer can be used other project PQR-If matching According the codes and new client requirements.
If yes, please provide code reference.

Thanks in Advance.
Best Regards,
Dominic.



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/650131b9-29c8-4683-b02f-cb6265988377%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMvP5sy3kEztvS77VUc_rGWikkUssop9482x_YwKwqDXbS50rw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...