Adding to it-"if End User or Service requirement states, then PWHT shall be required and to be identified in drawing or applicant documents".

Regards, Vino

On Nov 17, 2015 4:37 AM, "GrazG" <ing.grazianograsso@gmail.com> wrote:
I confirm for ASME B31.3-2014 all tickness of Group P1 the PWHT is not required. The only prescription is the PREHEAT at 95 °C for thickness >25 mm.
This is my interpretation, correct me if i'm wrong!

Il giorno martedì 1 settembre 2015 10:42:11 UTC+2, Mohd Siraj ha scritto:
Dear all,

As old ASME B31.3-2012  we know it was above 19mm req pwht,

now i read ASME B31.3-2014,little confused me with pwht exemption and pwht requirements and control thickenss 331.1.3?

q1- what is thik req for pwht for P1 as per b31.3 2014 ?

q2 : for P1,mentioned more than 25mm thk and 95C preheat exemption from pwht so less than 25mm not require pwht ?


regards,
mohd.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4133d41c-a4d9-46d7-b645-270688db2743%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7DMDz4g%2BFuC9tQ-gvfRXPki7ktjq6qYgTzdH2y%2BW0U5-g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...